When I do an overhang test, I always have this problem at about 35°. Does anyone have a suggestion what could be causing it?

  • Slicer: Orca
  • Layer height: 0.2mm
  • Infill: 0% (this has improved it a lot, I think the infill was causing bulging)
  • Outer walls: 2
  • Overhang speed: 10 or 20mm/s (both look the same)

Solution: I mistakenly thought overhang speed in Orca was based on overhang angle, it is percentage instead (which makes much more sense for different layer heights). My 10-25% overhang speed wasn’t set to slow down and that must translate to about 35° at 0.2mm layer height. I now have it set to 30mm/s and it now looks great 👍 And sorry, I was wrong when I stated the overhang speed 😅

    • Valmond@lemmy.world
      link
      fedilink
      English
      arrow-up
      5
      arrow-down
      1
      ·
      7 months ago

      I came here to say augment the print temperature! Look at those non binding “tubes” that are laid down every layer! They should melt into each other or it’s just crap and they’ll break under their own weight.

      Upping the fan is not needed here (yet, see below). It’s good when doing overhangs or printing without support and stuff start to sag down. When anything sags down probably :-)

      So up the temp for the overhangs, if they become too “liquid” then up the cooling(so fan speed).

      • UnH1ng3d@lemmy.worldOP
        link
        fedilink
        English
        arrow-up
        3
        ·
        7 months ago

        Thanks guys. I will try both and see what works. My layer adhesion is good / parts are strong though.

  • MotoAsh@lemmy.world
    link
    fedilink
    English
    arrow-up
    8
    arrow-down
    3
    ·
    7 months ago

    The corners are slowly curling up more and more until the nozzle goes completely outside of the curl and becomes an overhanged corner.

    The biggest problem is what ever is causing your plastic to curl while printing. Some plastics are terrible for it and you basically need a heated chamber to get rid of it. You could try playing with cooling settings or making a warmer environment, or … something else. Half the time if it’s a problem, I have to change the print or its orientation or add geometry so it doesn’t curl… It’s such a pain sometimes.

    • UnH1ng3d@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      3
      ·
      7 months ago

      Thanks. I’ll experiment with temperatures first but I’ve got some different filament on the way too as it happens, so hopefully I’ll manage to escape the problem one way or another 😁

    • rambos@lemm.ee
      link
      fedilink
      English
      arrow-up
      1
      ·
      7 months ago

      I thought curling as well, but I would expect that on higher angles instead. Its easy to confirm this if you watch the print. The solution would be lowering nozzle temp and slowing down the print (well, not less than 10 mm/s). I’ve seen that also too much cooling can cause curling, but thats for super strong part cooling

  • JoShmoe
    link
    fedilink
    English
    arrow-up
    3
    ·
    7 months ago

    Looks like the deformation is happening on the same layers where the overhangs of the number 35 are.

    • UnH1ng3d@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      3
      ·
      7 months ago

      It starts just underneath actually, but it still could be related 🤔 Maybe I need a test without numbers.

      • damium@programming.dev
        link
        fedilink
        English
        arrow-up
        4
        ·
        7 months ago

        If 35° (or something close to it) is the slicer setting for overhang detection it likely changes the cooling/speed/flow settings. If that is the case you can set it to a lower detection value and maybe get better results or change the normal cooling/speed/flow to be closer so it isn’t as drastic of a change.

        • UnH1ng3d@lemmy.worldOP
          link
          fedilink
          English
          arrow-up
          2
          ·
          7 months ago

          You may actually be right even though I thought I had checked this. Orca’s overhang speeds are based on overhang percentage and not angle, I previously just looked at the number and assumed it was degrees 🤦‍♂️I will match the speeds for all overhang percentage ranges and see if that solves it 🤞

        • UnH1ng3d@lemmy.worldOP
          link
          fedilink
          English
          arrow-up
          1
          ·
          7 months ago

          This was it! I had my 10-25% (not degrees 😅) overhang speed set not to slow down at all. I now have it set to 30mm/s and I have a perfect result. Thank you 👍😁

      • JoShmoe
        link
        fedilink
        English
        arrow-up
        1
        ·
        7 months ago

        I believe that if your layers are printing fast enough, the softer material would bend according to where the top layer is printed.

        • UnH1ng3d@lemmy.worldOP
          link
          fedilink
          English
          arrow-up
          1
          ·
          7 months ago

          Sorry, I didn’t follow that. Top layer of what? Not the actual top, top layer right?

          • JoShmoe
            link
            fedilink
            English
            arrow-up
            2
            ·
            7 months ago

            I meant, the next layer directly on top of where your deformed layers begin.